ISO 15614-8:2016-Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 8: Welding of tubes to tube-plate joints

ISO 15614-8:2016

ISO 15614-8:2016-Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 8: Welding of tubes to tube-plate joints

Format
Availability
Price and currency
Anglicky PDF
Immediate download
161.83 €
Francouzsky PDF
Immediate download
161.83 €
Anglicky Hardcopy
In stock
161.83 €
Francouzsky Hardcopy
In stock
161.83 €
Označení normy:ISO 15614-8:2016
Počet stran:18
Vydání:2
Vydáno:2016
DESCRIPTION

ISO 15614-8:2016


ISO 15614-8:2016 specifies requirements for the qualification testing of welding procedures for the arc welding of tube to tube-plate joints in metallic materials by manual, partly mechanized, fully mechanized, or automatic processes. ISO 15614-8:2016 is a part of a series of standards. Details of this series are given in ISO 15607, Annex A. Qualification by tube to tube-plate joint tests can be used for all joints even if they are fully loaded or only seal welded as required in application standards. ISO 15614-8:2016 applies to fusion welding of metallic materials for tube to tube-plate joints with a remaining gap between the tube and the tube-plate for some length of the tube-plate thickness. This part of ISO 15614 does not apply to tube-sheets with forged end connections with welded tubes (external/internal bore welds). For welding of tube to tube-plate joints with mechanical expansion which is load bearing, welding procedure test is to be defined. For other applications and/or requirements, this part of ISO 15614 can be used if required by the specification. Repair welding is to be considered in the welding procedure test.