ISO 16432:2006-Resistance welding — Procedure for projection welding of uncoated and coated low carbon steels using embossed projection(s)

ISO 16432:2006

ISO 16432:2006-Resistance welding — Procedure for projection welding of uncoated and coated low carbon steels using embossed projection(s)

Format
Availability
Price and currency
Anglicky PDF
Immediate download
116.34 €
Francouzsky PDF
Immediate download
116.34 €
Anglicky Hardcopy
In stock
116.34 €
Francouzsky Hardcopy
In stock
116.34 €
Označení normy:ISO 16432:2006
Počet stran:15
Vydání:1
Vydáno:2006
DESCRIPTION

ISO 16432:2006


ISO 16432:2006 specifies requirements for embossed-resistance-projection welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two thicknesses of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials: uncoated steels;hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;electrolytic zinc, zinc-iron, or zinc-nickel coated steel;aluminium coated steel;zinc-aluminium coated steel. Organic coated or primer coated steels are not covered by ISO 16432:2006.