UNE EN ISO 25239-4:2021
Friction stir welding - Aluminium - Part 4: Specification and qualification of welding procedures (ISO 25239-4:2020)
Soldeo por fricción-agitación. Aluminio. Parte 4: Especificación y cualificación de los procedimientos de soldeo. (ISO 25239-4:2020).
Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
118.27 €
Anglicky Hardcopy
In stock
118.27 €
Španělsky PDF
Immediate download
Printable
98.56 €
Španělsky Hardcopy
In stock
98.56 €
| Označení normy: | UNE EN ISO 25239-4:2021 |
| Počet stran: | 31 |
| Vydáno: | 2021-05-19 |
| Status: | Norma |
| Počet stran (Španělsky): | 33 |
DESCRIPTION
UNE EN ISO 25239-4:2021
This part of ISO 25239 specifies the requirements for the specification and qualification of welding procedures for the friction stir welding (FSW) of aluminium. In this document, the term aluminium refers to aluminium and its alloys. This document does not apply to friction stir spot welding which is covered by the ISO 18785- series. NOTE Service requirements, materials or manufacturing conditions can require more comprehensive testing than is specified in this document.