sklademVydáno: 2021-11-24
21/30415532 DC BS ISO 4680. Corrosion of metals and alloys. Method of uniaxial constant load test for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures

21/30415532 DC

BS ISO 4680. Corrosion of metals and alloys. Method of uniaxial constant load test for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures

CURRENCY
24.01 €
Označení normy:21/30415532 DC
Počet stran:37
Vydáno:2021-11-24
Status:Draft for Comment
DESCRIPTION

21/30415532 DC


This standard 21/30415532 DC BS ISO 4680. Corrosion of metals and alloys. Method of uniaxial constant load test for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures is classified in these ICS categories:
  • 77.060 Corrosion of metals