PRICES include / exclude VAT
This standard is no longer valid - contact us!
sklademVydáno: 2021-03-15
21/30427373 DC
BS EN ISO 11357-7. Plastics. Differential scanning calorimetry (DSC) Part 7. Determination of crystallization kinetics
CURRENCY
| Označení normy: | 21/30427373 DC |
| Počet stran: | 18 |
| Vydáno: | 2021-03-15 |
| Status: | Draft for Comment |
DESCRIPTION
21/30427373 DC
This standard 21/30427373 DC BS EN ISO 11357-7. Plastics. Differential scanning calorimetry (DSC) is classified in these ICS categories:
- 83.080.01 Plastics in general
This document specifies two methods (isothermal and non-isothermal) for studying the crystallisation kinetics of partially crystalline polymers using differential scanning calorimetry (DSC).
It is only applicable to molten polymers.
NOTE
These methods are not suitable if the molecular structure of the polymer is modified during the test.