PRICES include / exclude VAT
This standard is no longer valid - contact us!
sklademVydáno: 2023-03-22
23/30458743 DC
BS EN ISO 15614-13. Specification and qualification of welding procedures for metallic materials. Welding procedure test Part 13. Upset (resistance butt) and flash welding
CURRENCY
| Označení normy: | 23/30458743 DC |
| Počet stran: | 21 |
| Vydáno: | 2023-03-22 |
| Status: | Draft for Comment |
DESCRIPTION
23/30458743 DC
This standard 23/30458743 DC BS EN ISO 15614-13. Specification and qualification of welding procedures for metallic materials. Welding procedure test is classified in these ICS categories:
- 25.160.10 Welding processes