Main page>ASTM C1678-21R26 - Standard Practice for Fractographic Analysis of Fracture Mirror Sizes in Ceramics and Glasses
Vydáno: 01.06.2026

ASTM C1678-21R26

Standard Practice for Fractographic Analysis of Fracture Mirror Sizes in Ceramics and Glasses

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
188.00 €
Označení normy:ASTM C1678-21R26
Vydáno:01.06.2026
Status:Active
Počet stran:16
Sekce:15.01
Označení:ceramics; fractography; fracture mirror; fracture strength; fracture stress; fracture surface; glasses; hackle; microscope; mist; origin; residual stresses;
ASTM označení:ASTM C1678
Nahrazuje:C1678-21
DESCRIPTION

1.1 This practice pertains to the analysis and interpretation of fracture mirror sizes in brittle materials. Fracture mirrors (Fig. 1) are telltale fractographic markings that surround a fracture origin in brittle materials. The fracture mirror size may be used with known fracture mirror constants to estimate the stress in a fractured component. Alternatively, the fracture mirror size may be used in conjunction with known stresses in test specimens to calculate fracture mirror constants. The practice is applicable to glasses and polycrystalline ceramic laboratory test specimens as well as fractured components. The analysis and interpretation procedures for glasses and ceramics are similar, but they are not identical. Different optical microscopy examination techniques are listed and described, including observation angles, illumination methods, appropriate magnification, and measurement protocols. Guidance is given for calculating a fracture mirror constant and for interpreting the fracture mirror size and shape for both circular and noncircular mirrors including stress gradients, geometrical effects, residual stresses, or combinations thereof. The practice provides figures and micrographs illustrating the different types of features commonly observed in and measurement techniques used for the fracture mirrors of glasses and polycrystalline ceramics.

1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Související produkty
Anglicky Secure PDF
Immediate download
Non-printable
188.00 €
Anglicky Secure PDF Redline
Immediate download
Non-printable
208.00 €
Anglicky Secure PDF
Immediate download
Non-printable
188.00 €
Anglicky Secure PDF Redline
Immediate download
Non-printable
208.00 €