| Označení normy: | BS EN ISO 15610:2024 - TC |
| Počet stran: | 33 |
| Vydáno: | 2024-03-28 |
| ISBN: | 978 0 539 31223 2 |
| Status: | Tracked Changes |
DESCRIPTION
BS EN ISO 15610:2024 - TC
This standard BS EN ISO 15610:2024 - TC Tracked Changes. Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables is classified in these ICS categories:
- 25.160.10 Welding processes
- 25.030 Additive manufacturing