Main page>BS EN ISO 15614-6:2006 Specification and qualification of welding procedures for metallic materials. Welding procedure test Arc and gas welding of copper and its alloys
sklademVydáno: 2006-04-28
BS EN ISO 15614-6:2006 Specification and qualification of welding procedures for metallic materials. Welding procedure test Arc and gas welding of copper and its alloys

BS EN ISO 15614-6:2006

Specification and qualification of welding procedures for metallic materials. Welding procedure test Arc and gas welding of copper and its alloys

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
324.74 €
Anglicky Hardcopy
In stock
324.74 €
Označení normy:BS EN ISO 15614-6:2006
Počet stran:34
Vydáno:2006-04-28
ISBN:0 580 48158 1
Status:Standard
DESCRIPTION

BS EN ISO 15614-6:2006


This standard BS EN ISO 15614-6:2006 Specification and qualification of welding procedures for metallic materials. Welding procedure test is classified in these ICS categories:
  • 25.160.10 Welding processes

This part of ISO 15614 specifies how a preliminary welding procedure specification is qualified by welding procedure tests. It applies to the arc and gas welding of copper and copper alloys in all product forms.

This part of ISO 15614 defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of variables listed in Clause 9.

This part of ISO 15614 is applicable to all new welding procedures. However, it does not invalidate previous welding procedure tests made to former national standards or specifications. Where additional tests have to be carried out to make the qualification technically equivalent, it is only necessary to do the additional tests on a test piece made in accordance with this part of ISO 15614.

Additional tests may be required by application standards.

The principles of this part of ISO 15614 may be applied to other fusion welding processes.