Main page>BS EN ISO 204:2023 - TC Tracked Changes. Metallic materials. Uniaxial creep testing in tension. Method of test
sklademVydáno: 2023-09-06
BS EN ISO 204:2023 - TC Tracked Changes. Metallic materials. Uniaxial creep testing in tension. Method of test

BS EN ISO 204:2023 - TC

Tracked Changes. Metallic materials. Uniaxial creep testing in tension. Method of test

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
535.79 €
Anglicky Hardcopy
In stock
535.79 €
Označení normy:BS EN ISO 204:2023 - TC
Počet stran:144
Vydáno:2023-09-06
ISBN:978 0 539 28085 2
Status:Tracked Changes
DESCRIPTION

BS EN ISO 204:2023 - TC


This standard BS EN ISO 204:2023 - TC Tracked Changes. Metallic materials. Uniaxial creep testing in tension. Method of test is classified in these ICS categories:
  • 77.040.10 Mechanical testing of metals
This document specifies the methods for: a)    uninterrupted creep tests with continuous monitoring of extension; b)    interrupted creep tests with periodic measurement of elongation; c)    stress rupture tests where normally only the time to fracture is measured; d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported. NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.