Main page>BS ISO 18177:2025 Plastics. Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers. Differential scanning calorimetry (DSC)
sklademVydáno: 2025-05-15
BS ISO 18177:2025 Plastics. Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers. Differential scanning calorimetry (DSC)

BS ISO 18177:2025

Plastics. Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers. Differential scanning calorimetry (DSC)

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
284.84 €
Anglicky Hardcopy
In stock
284.84 €
Označení normy:BS ISO 18177:2025
Počet stran:30
Vydáno:2025-05-15
ISBN:978 0 539 24388 8
Status:Standard
DESCRIPTION

BS ISO 18177:2025


This standard BS ISO 18177:2025 Plastics. Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers. Differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.080.20 Thermoplastic materials