Main page>BS ISO 20579-4:2018 Surface chemical analysis. Guidelines to sample handling, preparation and mounting Reporting information related to the history, preparation, handling and mounting of nano-objects prior to surface analysis
sklademVydáno: 2018-04-24
BS ISO 20579-4:2018 Surface chemical analysis. Guidelines to sample handling, preparation and mounting Reporting information related to the history, preparation, handling and mounting of nano-objects prior to surface analysis

BS ISO 20579-4:2018

Surface chemical analysis. Guidelines to sample handling, preparation and mounting Reporting information related to the history, preparation, handling and mounting of nano-objects prior to surface analysis

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
276.42 €
Anglicky Hardcopy
In stock
276.42 €
Označení normy:BS ISO 20579-4:2018
Počet stran:32
Vydáno:2018-04-24
ISBN:978 0 580 90633 6
Status:Standard
DESCRIPTION

BS ISO 20579-4:2018


This standard BS ISO 20579-4:2018 Surface chemical analysis. Guidelines to sample handling, preparation and mounting is classified in these ICS categories:
  • 71.040.40 Chemical analysis

This document identifies information to be reported in a datasheet, certificate of analysis, report or other publication regarding the handling of nano-objects in preparation for surface chemical analysis. This information is needed to ensure reliability and reproducibility of analyses needed to advance research and technology using these materials, and for obtaining appropriate understanding of potential nano-object environmental and biological impacts. Such information is in addition to other details associated with specimen synthesis, processing history and characterization, and should become part of the data record (sometimes identified as provenance information) regarding the source of the material and changes that have taken place since it was originated.

This document includes informative annexes that summarize challenges associated with nano-objects that highlight the need for increased documentation and reporting in a material data record (Annex A) and provide examples of methods commonly used to extract particles from a solution for surface chemical analysis (Annex B). An example set of relevant sample data is shown in Annex C.

This document does not define the nature of instrumentation or operating procedures needed to ensure that the analytical measurements described have been appropriately conducted.