Main page>DIN EN 12814-3 Testing of welded joints of thermoplastics semi-finished products - Part 3: Tensile creep test
sklademDatum vydání: 2014-07
DIN EN 12814-3 Testing of welded joints of thermoplastics semi-finished products - Part 3: Tensile creep test

DIN EN 12814-3

Testing of welded joints of thermoplastics semi-finished products - Part 3: Tensile creep test

Prüfen von Schweißverbindungen aus thermoplastischen Kunststoffen - Teil 3: Zeitstand-Zugversuch

Format
Availability
Price and currency
Německy Hardcopy
In stock
107.40 €
Německy PDF
Immediate download
Printable
107.40 €
Anglicky Hardcopy
In stock
134.04 €
Anglicky PDF
Immediate download
Printable
134.04 €
Status:Norma
Datum vydání:2014-07
Označení:DIN EN 12814-3
Název produktu:Testing of welded joints of thermoplastics semi-finished products - Part 3: Tensile creep test
Počet stran:27
DESCRIPTION

DIN EN 12814-3