Main page>DIN EN ISO 11970 Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)
sklademDatum vydání: 2026-04
DIN EN ISO 11970 Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)

DIN EN ISO 11970

Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)

Schweißanweisungen für das Produktionsschweißen von Gussteilen auf Stahl- und Nickelbasis und deren Qualifizierung (ISO 11970:2025)

Format
Availability
Price and currency
Německy Hardcopy
In stock
107.40 €
Německy PDF
Immediate download
Printable
107.40 €
Anglicky Hardcopy
In stock
134.04 €
Anglicky PDF
Immediate download
Printable
134.04 €
Status:Norma
Datum vydání:2026-04
Označení:DIN EN ISO 11970
Název produktu:Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)
Počet stran:25
DESCRIPTION