PRICES include / exclude VAT
sklademDatum vydání: 2005-09
DIN EN ISO 15614-4
Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 4: Finishing welding of aluminium castings (ISO 15614-4:2005)
Anforderung und Qualifizierung von Schweißverfahren für metallische Werkstoffe - Schweißverfahrensprüfung - Teil 4: Fertigungsschweißen von Aluminiumguss (ISO 15614-4:2005)
Format
Availability
Price and currency
Německy Hardcopy
In stock
98.81 €
Německy PDF
Immediate download
Printable
98.81 €
Anglicky Hardcopy
In stock
123.36 €
Anglicky PDF
Immediate download
Printable
123.36 €
| Status: | Norma |
| Datum vydání: | 2005-09 |
| Označení: | DIN EN ISO 15614-4 |
| Název produktu: | Specification and qualification of welding procedures for metallic materials - Welding procedure test - Part 4: Finishing welding of aluminium castings (ISO 15614-4:2005) |
| Počet stran: | 20 |