Menu
0
Total price
0 €
PRICES include / exclude VAT
Main page>DIN EN ISO 204 Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)
sklademDatum vydání: 2023-10
DIN EN ISO 204 Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)

DIN EN ISO 204

Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)

Metallische Werkstoffe - Einachsiger Zeitstandversuch unter Zugbeanspruchung - Prüfverfahren (ISO 204:2023)

Format
Availability
Price and currency
Německy Hardcopy
In stock
176.52 €
Německy PDF
Immediate download
Printable
176.52 €
Anglicky Hardcopy
In stock
220.85 €
Anglicky PDF
Immediate download
Printable
220.85 €
Status:Norma
Datum vydání:2023-10
Označení:DIN EN ISO 204
Název produktu:Metallic materials - Uniaxial creep testing in tension - Method of test (ISO 204:2023)
Počet stran:58
DESCRIPTION

DIN EN ISO 204