>ISO 7539-5:1989-Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens
sklademVydáno: 1989
ISO 7539-5:1989-Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens

ISO 7539-5:1989

ISO 7539-5:1989-Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens

Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
73.83 €
Francouzsky PDF
Immediate download
Printable
73.83 €
Anglicky Hardcopy
In stock
73.83 €
Francouzsky Hardcopy
In stock
73.83 €
Označení normy:ISO 7539-5:1989
Počet stran:9
Vydání:1
Vydáno:1989
DESCRIPTION

ISO 7539-5:1989


Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.