>ISO 7539-5:1989 - Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens
sklademVydáno: 1989-12-07
ISO 7539-5:1989 - Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens

ISO 7539-5:1989

ISO 7539-5:1989 - Corrosion of metals and alloys — Stress corrosion testing — Part 5: Preparation and use of C-ring specimens

Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
Tisknutelné
1916 Kč
Francouzsky PDF
K okamžitému stažení
Tisknutelné
1916 Kč
Anglicky Tisk
Skladem
1916 Kč
Francouzsky Tisk
Skladem
1916 Kč
Označení normy:ISO 7539-5:1989
Vydání:1
Vydáno:1989-12-07
Počet stran (Anglicky):9
Počet stran (Francouzsky):9
Popis

ISO 7539-5:1989

Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.