PRICES include / exclude VAT
sklademVydáno: 2023-06-12
ISO 24087:2023
ISO 24087:2023 - Rubber, vulcanized — Determination of the glass transition temperature and enthalpy by differential scanning calorimetry
Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
118.70 €
Francouzsky PDF
Immediate download
Printable
118.70 €
Anglicky Hardcopy
In stock
118.70 €
Francouzsky Hardcopy
In stock
118.70 €
| Označení normy: | ISO 24087:2023 |
| Vydání: | 1 |
| Vydáno: | 2023-06-12 |
| Počet stran (Anglicky): | 13 |
| Počet stran (Francouzsky): | 13 |
DESCRIPTION
ISO 24087:2023
This document specifies a method of thermal analysis of vulcanized rubber by differential scanning calorimetry (DSC). This method is intended for the observation and measurement of various properties and phenomena associated, such as physical transitions (glass transition, melting and crystallization, polymorphic transitions, etc.).