>ISO 4680:2022 - Corrosion of metals and alloys — Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures
sklademVydáno: 2022-12-19
ISO 4680:2022 - Corrosion of metals and alloys — Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures

ISO 4680:2022

ISO 4680:2022 - Corrosion of metals and alloys — Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures

Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
187.14 €
Anglicky Hardcopy
skladem
187.14 €
Označení normy:ISO 4680:2022
Vydání:1
Vydáno:2022-12-19
Počet stran (Anglicky):27
DESCRIPTION

ISO 4680:2022

The document specifies a method for undertaking uniaxial constant load testing of the susceptibility of a metal, or an alloy, to stress corrosion cracking (SCC) in high-purity water environments at high temperature (above the boiling point of water at normal pressures) and pressure. The test method is particularly applicable to simulated primary water environments of light water reactors (LWRs).

The test method enables assessment of the relative resistance to SCC of a material in different environments and the comparative resistance of different materials (using the same environment, specimen dimensions and loading).

The terms “metal” and “alloy”, as used in the document, include weld metals and weld heat affected zones.