UNE EN 1902:2015
Adhesives - Test method for adhesives for floor and wall coverings - Shear creep test
Adhesivos. Métodos de ensayo de adhesivos para revestimientos de suelos y paredes. Ensayo de deformación progresiva por tensión de cizallamiento.
Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
67.27 €
Anglicky Hardcopy
In stock
67.27 €
Španělsky PDF
Immediate download
Printable
67.27 €
Španělsky Hardcopy
In stock
67.27 €
| Označení normy: | UNE EN 1902:2015 |
| Počet stran: | 13 |
| Vydáno: | 2015-10-21 |
| Status: | Norma |
| Počet stran (Španělsky): | 14 |
DESCRIPTION
UNE EN 1902:2015
This European Standard specifies a test method that gives an assessment of adhesion under long-term shear stress after bonding floor or wall coverings to a given substrate. The term wall covering does not include any type of wallpaper.