Main page>UNE EN ISO 11357-6:2026 - Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) (ISO 11357-6:2025)
sklademVydáno: 2026-02-25
UNE EN ISO 11357-6:2026 - Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) (ISO 11357-6:2025)

UNE EN ISO 11357-6:2026

Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) (ISO 11357-6:2025)

Plásticos. Calorimetría diferencial de barrido (DSC). Parte 6: Determinación del tiempo de inducción a la oxidación (OIT isotérmico) y de la temperatura de inducción a la oxidación (OIT dinámica). (ISO 11357-6:2025).

Format
Availability
Price and currency
Španělsky PDF
Immediate download
Printable
84.07 €
Španělsky Hardcopy
In stock
84.07 €
Anglicky PDF
Immediate download
Printable
84.07 €
Anglicky Hardcopy
In stock
84.07 €
Označení normy:UNE EN ISO 11357-6:2026
Počet stran:21
Vydáno:2026-02-25
Status:Norma
Počet stran (Španělsky):22
DESCRIPTION

UNE EN ISO 11357-6:2026

This document specifies methods for the determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT) of polymeric materials by means of differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized or compounded form, either as raw materials or finished products. It can be applicable to other plastics.