Main page>UNE EN ISO 11463:2021 - Corrosion of metals and alloys - Guidelines for the evaluation of pitting corrosion (ISO 11463:2020)
sklademVydáno: 2021-12-07
UNE EN ISO 11463:2021 - Corrosion of metals and alloys - Guidelines for the evaluation of pitting corrosion (ISO 11463:2020)

UNE EN ISO 11463:2021

Corrosion of metals and alloys - Guidelines for the evaluation of pitting corrosion (ISO 11463:2020)

Corrosión de metales y aleaciones. Directrices para la evaluación de la corrosión por picaduras. (ISO 11463:2020).

Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
84.00 €
Anglicky Hardcopy
In stock
84.00 €
Španělsky PDF
Immediate download
Printable
84.00 €
Španělsky Hardcopy
In stock
84.00 €
Označení normy:UNE EN ISO 11463:2021
Počet stran:21
Vydáno:2021-12-07
Status:Norma
Počet stran (Španělsky):22
DESCRIPTION

UNE EN ISO 11463:2021

This document provides guidance on the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.