Menu
0
Total price
0 €
PRICES include / exclude VAT
Main page>UNE EN ISO 11970:2026 - Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)
Vydáno: 2026-07-15
UNE EN ISO 11970:2026 - Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)

UNE EN ISO 11970:2026

Specification and qualification of welding procedures for production welding of steel and nickel-base castings (ISO 11970:2025)

Especificación y cualificación de procedimientos de soldeo para el soldeo de producción de moldeados de acero y a base de níquel. (ISO 11970:2025)

Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
92.13 €
Anglicky Hardcopy
In stock
92.13 €
Španělsky PDF
Immediate download
Printable
92.13 €
Španělsky Hardcopy
In stock
92.13 €
Označení normy:UNE EN ISO 11970:2026
Vydáno:2026-07-15
Status:Norma
Počet stran (Anglicky):26
Počet stran (Španělsky):29
DESCRIPTION

UNE EN ISO 11970:2026

This document specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. Tests are intended to be carried out in accordance with this document unless additional tests are specified by the purchaser or by agreement between the contracting parties. Previous procedure qualifications that conform to the range of qualification of Clause 8 are valid under this Document. Where additional tests have to be carried out to complete the qualification, it is only necessary to perform the additional tests to the requirements of Clauses 6 and 7. It defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables. This document applies to the arc welding of steel castings. The principles of this International Standard can be applied to other fusion welding processes subject to agreement between the contracting parties. In the case of specific service, material or manufacturing conditions, tests more comprehensive than those specified by this document can be specified by the purchaser, in order to gain more information, e.g. longitudinal weld tensile tests, bend tests, chemical analyses, ferrite determination in austenitic stainless steels, elongation after fracture, Charpy V-notch impact tests, and radiographic tests.

Categories: