UNE EN ISO 15610:2004
Specification and qualification of welding procedures for metallic materials - Qualification based on tested welding consumables (ISO 15610:2003)
Especificación y cualificación de procedimientos de soldeo para materiales metálicos. Cualificación basada en el empleo de consumibles de soldeo ensayados (ISO 15610:2003)
CURRENCY
| Označení normy: | UNE EN ISO 15610:2004 |
| Počet stran: | 11 |
| Vydáno: | 2004-07-16 |
DESCRIPTION
This standard UNE EN ISO 15610:2004 Specification and qualification of welding procedures for metallic materials - Qualification based on tested welding consumables (ISO 15610:2003) is classified in these ICS categories: