Menu
0
Total price
0 €
PRICES include / exclude VAT
Main page>BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test
sklademVydáno: 2008-06-30
BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

BS EN ISO 15324:2008

Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
Non-printable
196.77 €
Anglicky Hardcopy
In stock
196.77 €
Označení normy:BS EN ISO 15324:2008
Počet stran:14
Vydáno:2008-06-30
ISBN:978 0 580 60538 3
Status:Standard
DESCRIPTION

BS EN ISO 15324:2008


This standard BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test is classified in these ICS categories:
  • 77.060 Corrosion of metals