Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test
sklademVydáno: 2008-06-30
BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

BS EN ISO 15324:2008

Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS EN ISO 15324:2008
Počet stran:14
Vydáno:2008-06-30
ISBN:978 0 580 60538 3
Status:Standard
Popis

BS EN ISO 15324:2008


This standard BS EN ISO 15324:2008 Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test is classified in these ICS categories:
  • 77.060 Corrosion of metals