Main page>ISO 22848:2021 - Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
sklademVydáno: 2021-02-19
ISO 22848:2021 - Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

ISO 22848:2021

ISO 22848:2021 - Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

Format
Availability
Price and currency
Anglicky PDF
Immediate download
Printable
158.56 €
Anglicky Hardcopy
skladem
158.56 €
Označení normy:ISO 22848:2021
Vydání:1
Vydáno:2021-02-19
Počet stran (Anglicky):25
DESCRIPTION

ISO 22848:2021

This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.

The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.