Cena s DPH / bez DPH
sklademVydáno: 2021-02-19
ISO 22848:2021
ISO 22848:2021 - Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
Tisknutelné
3861 Kč
Anglicky Tisk
skladem
3861 Kč
| Označení normy: | ISO 22848:2021 |
| Vydání: | 1 |
| Vydáno: | 2021-02-19 |
| Počet stran (Anglicky): | 25 |
Popis
ISO 22848:2021
This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.
The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.