ASTM E2069-25

Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters on Cooling

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
1533 Kč
Anglicky Zabezpečené PDF Redline
K okamžitému stažení
Netisknutelné
1831 Kč
Anglicky Tisk
Skladem
1533 Kč
Označení normy:ASTM E2069-25
Vydáno:01.12.2025
Status:Active
Počet stran:7
Sekce:14.01
Označení:calibration; cooling; differential scanning calorimetry; temperature; thermal analysis;
ASTM označení:ASTM E2069
Nahrazuje:E2069-19
Popis

1.1 This test method describes the temperature calibration of differential scanning calorimeters (DSCs) on cooling using the difference between transition temperatures upon heating and cooling in the temperature range of 65 °C to 420 °C. Within this temperature range, an offset in the indicated temperature between heating and cooling experiments may be used to provide temperature calibration on cooling at other temperature ranges.

1.2 SI units are the standard. No other units of measurement are included in this standard.

1.3 Test Method E3142 is an alternative to this test method.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 6.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.