ISO 8993:2018-Anodizing of aluminium and its alloys — Rating system for the evaluation of pitting corrosion — Chart method
Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
2890 Kč
Francouzsky PDF
K okamžitému stažení
2890 Kč
Anglicky Tisk
Skladem
2890 Kč
Francouzsky Tisk
Skladem
2890 Kč
Označení normy: | ISO 8993:2018 |
Počet stran: | 12 |
Vydání: | 3 |
Vydáno: | 2018 |
Popis
ISO 8993:2018
This document specifies a chart rating system based on standard charts that provides a means of defining levels of performance of anodic oxidation coatings on aluminium and its alloys that have been subjected to corrosion tests. This rating system is applicable to pitting corrosion resulting from — accelerated tests, — exposure to corrosive environments, and — practical service tests. This document takes into account only pitting corrosion resulting from penetration of the protective anodic oxidation coating.