Cena s DPH / bez DPH
Hlavní stránka>22/30427287 DC BS EN ISO 15611. Specification and qualification of welding procedures for metallic materials. Qualification based on previous welding experience
Not available online - contact us!
sklademVydáno: 2022-07-21
22/30427287 DC BS EN ISO 15611. Specification and qualification of welding procedures for metallic materials. Qualification based on previous welding experience

22/30427287 DC

BS EN ISO 15611. Specification and qualification of welding procedures for metallic materials. Qualification based on previous welding experience

Měna
560 Kč
Označení normy:22/30427287 DC
Počet stran:12
Vydáno:2022-07-21
Status:Draft for Comment
Popis

22/30427287 DC


This standard 22/30427287 DC BS EN ISO 15611. Specification and qualification of welding procedures for metallic materials. Qualification based on previous welding experience is classified in these ICS categories:
  • 25.160.01 Welding, brazing and soldering in general