Cena s DPH / bez DPH
Hlavní stránka>22/30439293 DC BS ISO 7539-12. Corrosion of metals and alloys. Stress corrosion testing Part 12. Guidelines for atmospheric stress corrosion cracking testing
Not available online - contact us!
sklademVydáno: 2022-09-21
22/30439293 DC BS ISO 7539-12. Corrosion of metals and alloys. Stress corrosion testing Part 12. Guidelines for atmospheric stress corrosion cracking testing

22/30439293 DC

BS ISO 7539-12. Corrosion of metals and alloys. Stress corrosion testing Part 12. Guidelines for atmospheric stress corrosion cracking testing

Měna
560 Kč
Označení normy:22/30439293 DC
Počet stran:16
Vydáno:2022-09-21
Status:Draft for Comment
Popis

22/30439293 DC


This standard 22/30439293 DC BS ISO 7539-12. Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals