Cena s DPH / bez DPH
Hlavní stránka>ASTM E2602-22 - Standard Test Methods for Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry
Not available online - contact us!
Vydáno: 01.02.2022

E2602-22

Standard Test Methods for Assignment of the Glass Transition Temperature by Modulated Temperature Differential Scanning Calorimetry

Měna
1 253 Kč
Označení normy:E2602-22
Vydáno:01.02.2022
Status:Active
Počet stran:5
Sekce:14.01
Označení:cure; degree of cure; differential scanning calorimetry; glass transition temperature; modulated temperature differential scanning calorimetry; thermal analysis;
Popis

1.1 These test methods describe the assignment of the glass transition temperature of materials using modulated temperature differential scanning calorimetry (MTDSC) over the temperature range from –120 °C to +600 °C. The temperature range may be extended depending upon the instrumentation used.

1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.