Standard Practice for Calibration of Fixed-Cell Differential Scanning Calorimeters
Měna
| Označení normy: | E2603-15 |
| Vydáno: | 01.05.2015 |
| Status: | Active |
| Počet stran: | 5 |
| Sekce: | 14.01 |
| Označení: | calibration; differential scanning calorimetry; transition temperature; |
Popis
1.1 This practice covers the calibration of fixed-cell differential scanning calorimeters over the temperature range from –10 to +120°C.
1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 7.