F2625-10R16

Standard Test Method for Measurement of Enthalpy of Fusion, Percent Crystallinity, and Melting Point of Ultra-High-Molecular Weight Polyethylene by Means of Differential Scanning Calorimetry

Měna
1 138 Kč
Označení normy:F2625-10R16
Vydáno:01.04.2016
Status:Active
Počet stran:4
Sekce:13.02
Označení:crystallinity; differential scanning calorimetry; heat of fusion; melting temperature; thermal analysis; UHMWPE;
Popis

1.1 This test method discusses the measurement of the heat of fusion and the melting point of ultra-high-molecular weight polyethylene (UHMWPE), and the subsequent calculation of the percentage of crystallinity.

1.2 This test method can be used for UHMWPE in powder form, consolidated form, finished product, or a used product. It can also be used for irradiated or chemically-crosslinked UHMWPE.

1.3 This test method does not suggest a desired range of crystallinity or melting points for specific applications.

1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.