Cena s DPH / bez DPH
Hlavní stránka>BS EN 12814-3:2014 Testing of welded joints in thermoplastics semi-finished products Tensile creep test
sklademVydáno: 2014-02-28
BS EN 12814-3:2014 Testing of welded joints in thermoplastics semi-finished products Tensile creep test

BS EN 12814-3:2014

Testing of welded joints in thermoplastics semi-finished products Tensile creep test

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6960 Kč
Anglicky Tisk
Skladem
6960 Kč
Označení normy:BS EN 12814-3:2014
Počet stran:30
Vydáno:2014-02-28
ISBN:978 0 580 78955 7
Status:Standard
Popis

BS EN 12814-3:2014


This standard BS EN 12814-3:2014 Testing of welded joints in thermoplastics semi-finished products is classified in these ICS categories:
  • 25.160.40 Welded joints and welds

This European Standard specifies the dimensions, the method of sampling and the preparation of the test specimens, and the conditions for performing the tensile creep test perpendicular to the weld in order to determine the long-term tensile welding factor.

A tensile creep test may be used in conjunction with other tests (e.g. bend test, tensile test, macrographic examination, …) to assess the performance of welded assemblies, made from thermoplastics materials.

The test is applicable to welded assemblies made from thermoplastics materials filled or unfilled such as tubes and fittings, sheets, plates and profiles, but not reinforced, irrespective of the welding process used.