Cena s DPH / bez DPH
Hlavní stránka>BS EN 6041:2018 Aerospace series. Non-metallic materials. Test method. Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC)
sklademVydáno: 2018-02-12
BS EN 6041:2018 Aerospace series. Non-metallic materials. Test method. Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC)

BS EN 6041:2018

Aerospace series. Non-metallic materials. Test method. Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC)

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4980 Kč
Anglicky Tisk
Skladem
4980 Kč
Označení normy:BS EN 6041:2018
Počet stran:16
Vydáno:2018-02-12
ISBN:978 0 580 98578 2
Status:Standard
Popis

BS EN 6041:2018


This standard BS EN 6041:2018 Aerospace series. Non-metallic materials. Test method. Analysis of non-metallic materials (uncured) by Differential Scanning Calorimetry (DSC) is classified in these ICS categories:
  • 49.025.01 Materials for aerospace construction in general
This test method defines the procedure for the determination of the curing-characteristic and glass transition temperature of non-metallic materials (e.g. preimpregnated and neat resin systems, adhesives) for aerospace use by Differential Scanning Calorimetry (DSC). The results obtained by this method may be useful for: - derivation of the optimum cure cycle (only together with other test methods e.g. Tg determination) - assessment of the condition of the resin - assessment of the ageing behavior of the resin This European Standard does not give any directions necessary to meet the health and safety requirements. It is the responsibility of the user of this European Standard to adopt appropriate health and safety precautions.