BS EN ISO 11357-3:2025 - TC Tracked Changes. Plastics. Differential scanning calorimetry (DSC) Determination of temperature and enthalpy of melting and crystallization

BS EN ISO 11357-3:2025 - TC

Tracked Changes. Plastics. Differential scanning calorimetry (DSC) Determination of temperature and enthalpy of melting and crystallization

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6000 Kč
Anglicky Tisk
Skladem
6000 Kč
Označení normy:BS EN ISO 11357-3:2025 - TC
Počet stran:29
Vydáno:2025-06-18
ISBN:978 0 539 37420 9
Status:Tracked Changes
Popis

BS EN ISO 11357-3:2025 - TC


This standard BS EN ISO 11357-3:2025 - TC Tracked Changes. Plastics. Differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.080.01 Plastics in general
This document specifies a method for the determination of the temperatures and enthalpies of melting and crystallization of crystalline or partially crystalline plastics using conventional DSC as specified in ISO 11357-1. This document is not applicable to fast DSC as specified in ISO 23976.