Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 15609-5:2011 Specification and qualification of welding procedures for metallic materials. Welding procedure specification Resistance welding
sklademVydáno: 2012-03-31
BS EN ISO 15609-5:2011 Specification and qualification of welding procedures for metallic materials. Welding procedure specification Resistance welding

BS EN ISO 15609-5:2011

Specification and qualification of welding procedures for metallic materials. Welding procedure specification Resistance welding

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS EN ISO 15609-5:2011
Počet stran:22
Vydáno:2012-03-31
ISBN:978 0 580 77883 4
Status:Standard
Popis

BS EN ISO 15609-5:2011


This standard BS EN ISO 15609-5:2011 Specification and qualification of welding procedures for metallic materials. Welding procedure specification is classified in these ICS categories:
  • 25.160.10 Welding processes

This part of ISO 15609 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of this part of ISO 15609 to other resistance and related welding processes before any qualification is undertaken.

NOTE Details of ISO 15609 (all parts — for titles, see Foreword) are given in ISO 15607:2003, Annex A.

Variables listed in this part of ISO 15609 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.