BS EN ISO 15614-8:2016 Specification and qualification of welding procedures for metallic materials. Welding procedure test Welding of tubes to tube-plate joints

BS EN ISO 15614-8:2016

Specification and qualification of welding procedures for metallic materials. Welding procedure test Welding of tubes to tube-plate joints

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6728 Kč
Anglicky Tisk
Skladem
6728 Kč
Označení normy:BS EN ISO 15614-8:2016
Počet stran:32
Vydáno:2016-04-30
ISBN:978 0 580 85698 3
Status:Standard
Popis

BS EN ISO 15614-8:2016


This standard BS EN ISO 15614-8:2016 Specification and qualification of welding procedures for metallic materials. Welding procedure test is classified in these ICS categories:
  • 25.160.10 Welding processes