BS EN ISO 18785-4:2021 Friction stir spot welding. Aluminium Specification and qualification of welding procedures

BS EN ISO 18785-4:2021

Friction stir spot welding. Aluminium Specification and qualification of welding procedures

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS EN ISO 18785-4:2021
Počet stran:22
Vydáno:2021-01-26
ISBN:978 0 539 14166 5
Status:Standard
Popis

BS EN ISO 18785-4:2021


This standard BS EN ISO 18785-4:2021 Friction stir spot welding. Aluminium is classified in these ICS categories:
  • 25.160.10 Welding processes

This document specifies the requirements for the content of welding procedure specifications for the Friction Stir Spot welding (FSSW) of aluminium.

In this document, the term "aluminium" refers to aluminium and its alloys