Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 7500-2:2006 Metallic materials. Verification of static uniaxial testing machines Tension creep testing machines. Verification of the applied force
sklademVydáno: 2007-02-28
BS EN ISO 7500-2:2006 Metallic materials. Verification of static uniaxial testing machines Tension creep testing machines. Verification of the applied force

BS EN ISO 7500-2:2006

Metallic materials. Verification of static uniaxial testing machines Tension creep testing machines. Verification of the applied force

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6728 Kč
Anglicky Tisk
Skladem
6728 Kč
Označení normy:BS EN ISO 7500-2:2006
Počet stran:26
Vydáno:2007-02-28
ISBN:978 0 580 50137 1
Status:Standard
Popis

BS EN ISO 7500-2:2006


This standard BS EN ISO 7500-2:2006 Metallic materials. Verification of static uniaxial testing machines is classified in these ICS categories:
  • 77.040.10 Mechanical testing of metals

This part of ISO 7500 specifies the verification of testing machines used for uniaxial creep testing in tension in accordance with ISO 204.

The verification consists of

  • a general inspection of the testing machine, and

  • a verification of the force applied by the testing machine.

This part of ISO 7500 applies to dead-weight machines, lever-type creep testing machines and direct-spring-loading machines.

Machines with a force-measuring system1) should be verified in accordance with ISO 7500-1, Metallic materials - Verification of static uniaxial testing machines - Part 1: Tension/compression testing machines - Verification and calibration of the force-measuring system.