Cena s DPH / bez DPH
sklademVydáno: 1994-10-01
BS EN ISO 7539-3:1995
Corrosion of metals and alloys. Stress corrosion testing Preparation and use of U-bend specimens
Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4260 Kč
Anglicky Tisk
Skladem
4260 Kč
| Označení normy: | BS EN ISO 7539-3:1995 |
| Počet stran: | 12 |
| Vydáno: | 1994-10-01 |
| ISBN: | 0 580 18793 4 |
| Status: | Standard |
Popis
BS EN ISO 7539-3:1995
This standard BS EN ISO 7539-3:1995 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
- 77.060 Corrosion of metals
Procedures for designing, preparing and using U-bend test specimens for investigating the susceptibility of a metal to stress corrosion.