Cena s DPH / bez DPH
Hlavní stránka>BS ISO 14322:2018 Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)
sklademVydáno: 2018-07-20
BS ISO 14322:2018 Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

BS ISO 14322:2018

Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4980 Kč
Anglicky Tisk
Skladem
4980 Kč
Označení normy:BS ISO 14322:2018
Počet stran:18
Vydáno:2018-07-20
ISBN:978 0 580 51669 6
Status:Standard
Popis

BS ISO 14322:2018


This standard BS ISO 14322:2018 Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.080.10 Thermosetting materials

This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.

This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.