Cena s DPH / bez DPH
Hlavní stránka>BS ISO 15309:2013 Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices
sklademVydáno: 2013-12-31
BS ISO 15309:2013 Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

BS ISO 15309:2013

Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS ISO 15309:2013
Počet stran:18
Vydáno:2013-12-31
ISBN:978 0 580 74909 4
Status:Standard
Popis

BS ISO 15309:2013


This standard BS ISO 15309:2013 Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices is classified in these ICS categories:
  • 11.040.40 Implants for surgery, prosthetics and orthotics

This International Standard specifies a method for the thermal analysis of Poly Ether Ether Ketone (PEEK) that is for use in the manufacture of implantable medical devices, using differential scanning calorimetry (DSC).

The transition temperatures to be determined are the glass transition temperature (Tg), the melting temperature (Tm) and the crystallization temperature on cooling (Tc).