Cena s DPH / bez DPH
Hlavní stránka>BS ISO 16540:2015 Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method
sklademVydáno: 2015-10-31
BS ISO 16540:2015 Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method

BS ISO 16540:2015

Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6960 Kč
Anglicky Tisk
Skladem
6960 Kč
Označení normy:BS ISO 16540:2015
Počet stran:30
Vydáno:2015-10-31
ISBN:978 0 580 73641 4
Status:Standard
Popis

BS ISO 16540:2015


This standard BS ISO 16540:2015 Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method is classified in these ICS categories:
  • 77.060 Corrosion of metals

This International Standard provides guidelines for the use of four-point bend testing to evaluate the resistance of metals including carbon steel, low alloy steels, and corrosion resistant alloys (CRAs) to stress corrosion cracking. The method gives guidance on testing of both parent plate and welds and includes procedures for metals that have no distinct yield point in their stress-strain behaviour as well as metals with a distinct yield point. The emphasis in this International Standard is on the generic methodology of the four-point bend test. Service application will be varied and the relevant industry standard is to be consulted where appropriate.