Hlavní stránka>BS ISO 18373-2:2008 Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the enthalpy of fusion of crystallites
sklademVydáno: 2008-03-31
BS ISO 18373-2:2008 Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the enthalpy of fusion of crystallites

BS ISO 18373-2:2008

Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the enthalpy of fusion of crystallites

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS ISO 18373-2:2008
Počet stran:20
Vydáno:2008-03-31
ISBN:978 0 580 57185 5
Status:Standard
Popis

BS ISO 18373-2:2008


This standard BS ISO 18373-2:2008 Rigid PVC pipes. Differential scanning calorimetry (DSC) method is classified in these ICS categories:
  • 23.040.20 Plastics pipes

This part of ISO 18373 specifies a method for the determination of the enthalpy of fusion of crystallites in rigid PVC pipe samples. The method is based on the measurement of the thermal history using differential scanning calorimetry (DSC) and is suitable for all types of rigid PVC pipes.