BS ISO 22768:2020 Raw rubber and rubber latex. Determination of the glass transition temperature by differential scanning calorimetry (DSC)

BS ISO 22768:2020

Raw rubber and rubber latex. Determination of the glass transition temperature by differential scanning calorimetry (DSC)

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
4814 Kč
Anglicky Tisk
Skladem
4814 Kč
Označení normy:BS ISO 22768:2020
Počet stran:18
Vydáno:2020-07-15
ISBN:978 0 539 05964 9
Status:Standard
Popis

BS ISO 22768:2020


This standard BS ISO 22768:2020 Raw rubber and rubber latex. Determination of the glass transition temperature by differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.060 Rubber
  • 83.040.10 Latex and raw rubber

This document specifies a method using a differential scanning calorimeter to determine the glass transition temperature of raw rubber and rubber latex.