Cena s DPH / bez DPH
Hlavní stránka>BS ISO 22848:2021 Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
sklademVydáno: 2021-02-24
BS ISO 22848:2021 Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

BS ISO 22848:2021

Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
Netisknutelné
6728 Kč
Anglicky Tisk
Skladem
6728 Kč
Označení normy:BS ISO 22848:2021
Počet stran:32
Vydáno:2021-02-24
ISBN:978 0 580 51813 3
Status:Standard
Popis

BS ISO 22848:2021


This standard BS ISO 22848:2021 Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water is classified in these ICS categories:
  • 77.060 Corrosion of metals

This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.

The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.